1、Microstructure of working layer in the barrel: pearlite or tempered sorbite.

sorbite造句

2、The results show that X80 pipeline steel obtains sorbite after quenching and tempering, gets pearlite by normalizing.

3、With the decrease of finishing rolling temperature, the grain size is refined apparently and the contents of sorbite is increased.

4、The results indicated that the tempered sorbite was the optimum microstructure, the inhomogeneous distribution of micro hardness affected markedly the finish quality of the steel surface.

5、The results show that 82b wire rod brittle fracture is mainly caused by excessive inclusion, reticulate carbide, lower sorbite in the microstructure, and surface defect of wire rod.